RTV_111

EPUSIL U 232

 

General purpose, electrical potting and casting

Self-Extinguishing Urethane compound   

 

DESCRIPTION

Epusil U 232 is a unique, moderate viscosity, two components fast curing polyurethane casting compound.  The cured compound exhibits high physical and electrical properties even at elevated temperatures. Epusil U 232 is UL 94 V-0 standard approved.

 

PROPERTIES - Uncured

Part A                                    Part B

Viscosity, cps @ 250C ....................      6000+/-1000                              100-150

Specific Gravity g/cm3 ....................      1.5 +/-0.03                                1.2

Mix Ratio (weight) ..........................                             100:20

Mixed Viscosity ...............................                            3500-4000

Mixed Specific Gravity g/cm3 ..........                              1.45+/-0.04

Gel Time @ 250C, min ....................                              20

De-mold Time 250C, hr ...................                              3-4

Ultimate Cure 250C days ..................                            7-8

Shelf Life 250C, months ...................     6                                              6

 

PROPERTIES - Cured

Hardness, Shore D .............................                          65-70

Tensile Strength kg/cm2  .................…                           275 +/- 10

Tensile Elongation % ......................…                          3.7  +/- 0.2

Compressive Strength kg/cm2 ........…..                          420 - 440 

Water Absorption % ........................…                         < 0.2

Flammability Rating ...........................                           UL 94 - V - 0

Working temperature 0C ....................                           100

 

ELECTRICAL

Dielectric Strength kV/mm ..................                          18

Dielectric Constant ...............................                        4.0

Dissipation Factor ................................                         0.030

Volume Resistivity, Ohm-cm  .......….....                        3*1014

Thermal Conductivity, W/ m0C ......…...                         0.8


 

MIXING INSTRUCTION

1.      Pre mix Epusil U 232 in the original container.

2.      Weigh out the required amount of part A.

3.      Weigh into 100 parts of Part A 20 parts of Part B.

4.      Mix thoroughly scraping both sides and bottom of the mixing container.

5.   Pour into mold.