DESCRIPTION

Epusil RTV 185 is high tear strength, high elongation cur RTV Silicone rubber.

Properties - Uncured

Part A                                      Part B

Color, visual ..........................…..        White                                       Transparent

Viscosity  (cps @ 250C)...…...…..       35000 to 45000                       250

Specific Gravity (gr/cm3 @ 250C).        1.2                                           1.05

Mix Ratio (weight) ..........……..….                               100:5

Mix viscosity  (cps @ 250C).……...                             30000-35000

Pot life @ 250C ....................……..                             2.5-3 hours      

Shelf life @ 250C (months)...………    6                                              6

Properties - Cured

Physical

Hardness, Shore A ..............………    35-40

Tensile Strength kg/cm .......………      48-53

Tensile Elongation  % ..........……..       200+/- 20

Tear Strength (Die B kg/cm2)....….      25 +/- 2

Service temperature ............……….    -50 to 2000C

Mixing Instructions

1.        Pre-mix RTV 185 Part A in its original container.

2.        Weigh out required amount of part A. Weight into 5 parts oh Part B (catalyst) for each 100 parts of Part A (base)

3.        Mix thoroughly, scraping both the bottom and side of the mixing container.

4.        Place in a vacuum chamber and draw about 29 inches of mercury. The mixture will rise to about 3-4 times the original volume, then collapse. Hold the vacuum for another 4 to 5 minutes and release.

Proceed to pour mold. 